C Mn P S Al
≤0.15 ≤0.60 ≤0.100 ≤0.050 ≥0.02
Yield Strength Mpa Tensile Strength Mpa Elongation(Thickness)
≤280 270-410 ≥28

C Mn P S Al
≤0.10 ≤0.45 ≤0.045 ≤0.045 ≥0.02
Yield Strength Mpa Tensile Strength Mpa Elongation(Thickness)
≤240 270-370 ≥34
C Mn P S Al
≤0.08 ≤0.40 ≤0.030 ≤0.030 ≥0.02
Yield Strength Mpa Tensile Strength Mpa Elongation(Thickness)
≤210 270-350 ≥38
C Mn P S Al
≤0.06 ≤0.35 ≤0.025 ≤0.025 ≥0.015
Yield Strength Mpa Tensile Strength Mpa Elongation(Thickness)
≤180 270-330 ≥40
C Mn P S Al
≤0.02 ≤0.30 ≤0.020 ≤0.020 ≥0.015
Yield Strength Mpa Tensile Strength Mpa Elongation(Thickness)
≤170 270-330 ≥41

C Mn P S Al
≤0.01 ≤0.25 ≤0.020 ≤0.020 ≥0.015
Yield Strength Mpa Tensile Strength Mpa Elongation(Thickness)
≤150 250-310 ≥44