ASTM A131 Grade EH40
Grade ASTM A131 EH40 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥390 510-650 ≥19 ≥22 37 -40
ASTM A131 Grade FH40
Grade ASTM A131 FH40 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.16 0.10-0.50 0.90-1.60 0.025 0.025 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 0.009
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥390 510-650 ≥19 ≥22 37 -60
ASTM A131 Grade AH40
Grade ASTM A131 AH40 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥390 510-650 ≥19 ≥22 37 0
ASTM A131 Grade DH40
Grade ASTM A131 DH40 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥390 510-650 ≥19 ≥22 31 -20
ASTM A131 Grade EH36
Grade ASTM A131 EH36 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥355 490-620 ≥19 ≥22 34 -40
ASTM A131 Grade FH36
Grade ASTM A131 FH36 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.16 0.10-0.50 0.90-1.60 0.025 0.025 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 0.009
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥355 490-620 ≥19 ≥22 37 -60
ASTM A131 Grade AH36
Grade ASTM A131 AH36 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥355 490-620 ≥19 ≥22 34 0
ASTM A131 Grade DH36
Grade ASTM A131 DH36 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥355 490-620 ≥19 ≥22 34 -20
ASTM A131 Grade EH32
Grade ASTM A131 EH32 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥355 440-590 ≥19 ≥22 31 -40
ASTM A131 Grade FH32
Grade ASTM A131 FH32 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.16 0.10-0.50 0.90-1.60 0.025 0.025 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 0.009
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥315 440-590 ≥19 ≥22 31 -60
ASTM A131 Grade AH32
Grade ASTM A131 AH32 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥315 440-590 ≥19 ≥22 31 0
ASTM A131 Grade DH32
Grade ASTM A131 DH32 C % Si % Mn % P % S % Al(acid soluble),min% Cb V Ti Cu Cr Ni Mo N
0.18 0.10-0.50 0.90-1.60 0.035 0.035 0.015 0.02-0.05 0.05-0.10 0.02 0.35 0.20 0.40 0.08 -
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥315 440-590 ≥19 ≥22 31 -20
ASTM A131 Grade D
Grade ASTMA131 D C % Si % Mn.Min % P % S % C+Mn/6
0.21 0.10-0.35 0.60 0.035 0.035 0.40
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥235 400-520 ≥21 ≥24 27 -20
ASTM A131 Grade E
Grade ASTMA131 E C % Si % Mn.Min % P % S % C+Mn/6
0.18 0.10-0.35 0.70 0.035 0.035 0.40
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥235 400-520 ≥21 ≥24 27 -40
ASTM A131 Grade B
Grade ASTMA131 B C % Si % Mn.Min % P % S % C+Mn/6
0.21 0.35 0.60 0.035 0.035 0.40
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥235 400-520 ≥21 ≥24 27 0
ASTM A131 Grade A
Grade ASTMA131 A C % Si % Mn.Min % P % S % C+Mn/6
0.21 0.50 2.5xC 0.035 0.035 0.40
Yield Strength (Mpa) Tensile Strength (MPa) Elongation in8 in.[200mm] (%) Elongation in8 in.[200mm] (%) Impact Energy (J) Test Temperature(°C)
≥235 400-520 ≥21 ≥24 27 20