Shipbuilding Plate API Spec 2H
Grade | C % max | Mn % | P % max | S% | Si% | Nb | Ti | Al | N max | V |
2HGr42 | 0.18 | 0.90-1.35 | 0.030 | 0.010 | 0.05-0.40 | ≤ 0.04 | ≤0.02 | 0.02-0.06 | 0.012 | d |
Grade |
Yield Strength,kis (Mpa) min |
Tensile Strength,kis (MPa) |
Elongation (%)min |
2HGr42 | t≤2.5in 42(289) t≥2.5in 42(289) | 62-82(427-565) |
2in.(50mm) 22 8in.(200mm) 18 |
Grade | C % max | Mn % | P % max | S% | Si% | Nb | Ti | Al | N max | V |
2HGr50 | 0.18 | 0.15-1.60 | 0.030 | 0.010 | 0.05-0.40 | 0.01-0.04 | ≤0.02 | 0.02-0.06 | 0.012 | d |
Grade |
Yield Strength,kis (Mpa) min |
Tensile Strength,kis (MPa) |
Elongation (%)min |
2HGr50 | t≤2.5in 50(345)t≥2.5in 47(324) | 70-90(483-620) |
2in.(50mm) 21 8in.(200mm) 16 |
If you are interested in other shipbulinding steel plates, please click - ASTM A131, ABS Ship Class, CCS Ship Class, LR Ship Class, DNV Ship Class, BV Ship Class, GL Ship Class, RINA Ship Class, KR Ship Class, NK Ship Class, EN10225, API Spec 2H.
- NM400 steel plate
- low alloy steel plate
- Cor-Ten steel plate
- stainless steel plate
- pipeline steel plate
- pressure vessel steel plate
- abrasion resistant steel plate
- shipbuilding steel plate
- steel coil
- carbon steel plate
- Cold rolled steel coil
- testing
- quality policy Steel Grades
- EN 10130 cold rolled steel coil specification
- GB/T5213 - 2008 cold rolled coil
- JIS G3141 steel coil specification
- NM500 wear resistant steel
- NM450 wear resistant steel